dc.date.accessioned | 2014-02-13T11:08:55Z | |
dc.date.available | 2014-02-13T11:08:55Z | |
dc.date.issued | 2013 | en_US |
dc.date.submitted | 2013-06-02 | en_US |
dc.identifier.citation | Skott, Aina Øverås. High Temperature Oxidation of Sanergy HT - oxidation kinetics and growth mechanism of a metallic interconnect. Masteroppgave, University of Oslo, 2013 | en_US |
dc.identifier.uri | http://hdl.handle.net/10852/38252 | |
dc.language.iso | eng | en_US |
dc.title | High Temperature Oxidation of Sanergy HT - oxidation kinetics and growth mechanism of a metallic interconnect | en_US |
dc.type | Master thesis | en_US |
dc.date.updated | 2014-02-11 | en_US |
dc.creator.author | Skott, Aina Øverås | en_US |
dc.subject.nsi | VDP::440 | en_US |
dc.identifier.bibliographiccitation | info:ofi/fmt:kev:mtx:ctx&ctx_ver=Z39.88-2004&rft_val_fmt=info:ofi/fmt:kev:mtx:dissertation&rft.au=Skott, Aina Øverås&rft.title=High Temperature Oxidation of Sanergy HT - oxidation kinetics and growth mechanism of a metallic interconnect&rft.inst=University of Oslo&rft.date=2013&rft.degree=Masteroppgave | en_US |
dc.identifier.urn | URN:NBN:no-40815 | |
dc.type.document | Masteroppgave | en_US |
dc.identifier.duo | 182040 | en_US |
dc.identifier.fulltext | Fulltext https://www.duo.uio.no/bitstream/handle/10852/38252/1/Skott.pdf | |